NDT not required for pipe support as per AWS D 1.1 unless not touch with piping weld joint.
 
Thank you & Best Regards,
________________________________________
Dinesh Ravi Shankar,
+ Email: dinesh_ravi2001@yahoo.com,
È +91 9566436626 | +91 9944665579.



On Tuesday, June 6, 2017 5:12 PM, Dinesh Patil <dinn.patil@gmail.com> wrote:


Dear All,

Can you please tell me whether NDT is require OR not for pipe support weld.

If yes then where it is mentioned means which clause in AWS D1.1

Thank you

DINESH
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...