Saturday, June 3, 2017

Re: [MW:26574] Re: P1-P1 qualified WPS for welding API 5L PSL2

Dear friend,

 You can use E6010 for root and E7018 for other passes, Otherwise check your Tender specification

On Thu, Jun 1, 2017 at 11:48 AM, jiju balan <jj@arcube.in> wrote:
dear team,
what electrode should be used to weld  API 5L GR-B PSL1 pipes.

regards

On Wednesday, January 2, 2013 at 5:32:43 PM UTC+5:30, krishna wrote:
Dear Team,

We have WPS/PQR for SA106 Gr.B(P1-P1) whether this shall be used for welding of API 5L PSL2
seamless & welded pipes for production and welder qualification.

pls share your experiences.

thanks,
krishna

Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Thanks & regards

Anish S 

Sr.Engineer-QA/QC

Corrtech International Pvt Ltd

Kochi

Mob: +91 9442938358

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...