Re: [MW:26590] NDT Requirement

NDT not required for pipe support as per AWS D 1.1 unless not touch with piping weld joint.
 
Thank you & Best Regards,
________________________________________
Dinesh Ravi Shankar,
+ Email: dinesh_ravi2001@yahoo.com,
È +91 9566436626 | +91 9944665579.



On Tuesday, June 6, 2017 5:12 PM, Dinesh Patil <dinn.patil@gmail.com> wrote:


Dear All,

Can you please tell me whether NDT is require OR not for pipe support weld.

If yes then where it is mentioned means which clause in AWS D1.1

Thank you

DINESH
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...