First 2 terms used when two or tendam wire feeder used in same time of welding with fast welding multibead welding.
3 point orientation of wire with respect to workpiece
.
Thanking You,
With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135
On Jun 21, 2017 6:38 PM, "nguyen tuan" <tuanpvecc@gmail.com> wrote:
-- Dear Expert--Now I am preparing WPS for SAW as per AWS D1.1Please explain the welding terms for SAW process1. Longitudinal Spacing of Arc2. Lateral Spacing of Arc3. Angle of Electrode.Thank you in advanceBest Regards,Tuan
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments