Dear ;
You can use for API 5L Gr B , E6010 for penetration and E 7018 for filling and cap.
regards
Le Jeudi 1 juin 2017 6h27, jiju balan <jj@arcube.in> a écrit :
dear team,
what electrode should be used to weld API 5L GR-B PSL1 pipes.
regards
On Wednesday, January 2, 2013 at 5:32:43 PM UTC+5:30, krishna wrote:
-- what electrode should be used to weld API 5L GR-B PSL1 pipes.
regards
On Wednesday, January 2, 2013 at 5:32:43 PM UTC+5:30, krishna wrote:
Dear Team,
We have WPS/PQR for SA106 Gr.B(P1-P1) whether this shall be used for welding of API 5L PSL2
seamless & welded pipes for production and welder qualification.
pls share your experiences.
thanks,
krishna
Catch India as it happens with the Rediff News App. To download it for FREE, click here
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments