Friday, June 2, 2017

[MW:26572] Re: Hardness survey requirement to NACE MR 0175.

Dear,

Pl read NACE SP0472 which answers your query.

On Saturday, May 27, 2017 at 10:58:40 AM UTC+5:30, Baskaran wrote:
Dear Experts,

Please advise on below query.

Applicable code are;
ASME Section IX
NACE MR 0175.

We have one WPS Qualified in butt joint and Hardness survey done  according to NACE MR 0175 (7.3.3.3 Figure 2)  on Butt weld coupon.

​Is it correct that we cannot use the above WPS in a fillet joint because the fillet weld hardness survey is not carried out.

​Thanks.​
Bas

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...