Thursday, June 15, 2017

Re: [MW:26613] API 650 Fuel Tanks repair - Hydro test

Yes

Paint covered on the weld lines shall be removed before hydro test



From: Maulik Dodiya <maulik.dodiya@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, June 15, 2017 9:12 AM
Subject: [MW:26612] API 650 Fuel Tanks repair - Hydro test

Dear All,

Can anyone share info. regarding Hydro test procedure during steel repair of Fuel storage tanks? Do we need to remove existing paint completely before Hydro test ? Please advise.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...