Re: [MW:26597] Electrode for Buttered Alloy Steel With H2S carbon Steel Material

Hi

You can select the filler wire ERNiCrMo3 or electrode ENiCrMo-3.

Please share me the exact material specification of inconel for review.

Regards
P Govindan

On Jun 7, 2017 07:21, "'Mostafa Kamel Hussein' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Dears
Can you please provide me with compatible electrode which will be utilized to weld carbon steel (H2S) material with A335-P11 butting with inconel?
As you know i can NOT select any nickel electrode due to high Ni% which is prevented in case of (H2S) as per project specification

your feedback is highly recommended

Regards,
M.Kamel

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...