Wednesday, June 7, 2017

Re: [MW:26596] NDE requirements for oil piping (tubing) - Mechanical equipments

Dear Gents,
Oil line can do hydrotest . Since it is non boiler external piping-follow ASME 31.3 Code.



On Jun 6, 2017 6:59 PM, "Zakaria ghrab" <zakaria.ghrab@gmail.com> wrote:
Dear all,

  Could you please advice:

- Project : Power plant construction project
- Construction code ASME B31.1

Query : Oil piping (tubing) for mechnaical equipments (Fans,...) : 
-  Any ASME or API related code/standard ?
- code for construction, welding and NDE ?
- Pressure test : is it mandatory ? Pneumatic or just oil flushing 


Thank you for your support.

--

Thanks and Regards, 
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805
Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...