Friday, June 9, 2017

Re: [MW:26601] use of CS replace of LTCS

Hi
We can not use CS in place of LTCS, project design has to approve.

Regards
GOVIN

On Jun 9, 2017 09:58, "abdulkhadar musthafa" <abdulrilvan@gmail.com> wrote:
Dear Experts

We can use of CS replace of LTCS???

--
ABDUL KHADAR MUSTHAFA
QC-WELDING INSPECTOR
+91-9841879981
"The reward of deeds depends upon the intentions"
"செயல்கள் அனைத்தும் எண்ணங்களைப் பொருத்தே அமைகின்றன. ஒவ்வொருவருக்கும் அவர் எண்ணியதே கிடைக்கிறது."


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...