Thursday, June 22, 2017

Re: [MW:26633] Cast Iron to MS Welding

ENiFe-CI

On 22-Jun-2017 2:26 PM, "Amit Singh" <amit086@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (amit086@gmail.com) Add cleanup rule | More info

Dear Experts,

Please suggest a suitable welding electrode to join Cast Iron to MS plate inside the boiler.

Maximum temp inside the boiler is approx 400 deg C.

Thank you in advance.

Regards,

Amit Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...