Dear expert ,

We have a two times repaired joint , This joints is cutted in order to peform hydrotest and welded again ( golden joints ).
That means this joint is welded 4 times : initial weld , first repair , second repair and golden weld repair .
My question is : ther is any limitation for repair numebr for one joint , if yes please give reference ? the mechanical proprities for HAZ are same after all this repair ?