Re: [MW:26616] WQT- Electrode

Yes, your observation is a valid one.
Generally 7010 is not for fill pass however pls check the WPS once and discuss in detail with the person who proposed for 7010 for this application.
Better to understand their perspective also.

Thanks and Regards
Lakshmankumar B
9440031459

Sent from my iPhone

On 13-Jun-2017, at 1:14 PM, Shankar S <sshankar.irs@gmail.com> wrote:

Dear experts,

At one particular LPG bottling plant contractor proposed  WQT approval root run as E6010 and fill as E7010.  I have doubt that E7018 is suppose use for fill up only. 

Project: Pipeline. Pipe specification PSL2( API)-  Oil & Gas. Ref. standards: API 1104, ASME B 31.4/8.

Please suggest accordingly.

Thanks in Advance.

regards,
Shankar
Hyderabad India.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...