Stick to permissible variation in flat surface as defined in ASTM A20 as API stipulates nearly as possible a plane surface (7.2.2.1)
On Mon, Jun 12, 2017 at 3:04 PM, Aneesh <aneeshknair87@gmail.com> wrote:
Dear All
Can anyone share the acceptance criteria for annular or bottom plate distortion that had happened due to welding of for API 650 atmospheric Tanks.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments