Re: [MW:26567] ASME B31.3 -2014 Table 331.1.1 Soaking time for P1 material

Dear,
For your information the latest edition ASME B31.3 says there is no any requirements of PWHT.
If the wall thickness is more then will do preheat @95 Deg Celsius and which exemption of PWHT.

Regards,
Rajendra Jadhav

On 29-May-2017 3:33 PM, "SWI" <tulasiramus@gmail.com> wrote:
Hi Team,

Could any please clarify
What is the minimum required soaking time for P1 material with wall thick 12mm, as per ASME B31.3 year 2014 Table 331.1.1 .

Is it still Minimum one hour per 1 Inch wall thickness or Minimum 15 Minutes...


Regards,

Ram

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...