[MW:26602] Welder Qualification according to API 1104

Dear Gents,

According to API 1104. Is it possible to qualify a welder by testing "on the job" ? The welder already qualified on 5G position, can I test that welder on 6G position during production, I mean consider the first 6G joint as WQT. 


Thanks in advance.

Regards.
Shaban



--