[MW:26565] Re: ASME B31.3 -2014 Table 331.1.1 Soaking time for P1 material

For P no. 1 & 12 mm, the minimum soaking time for PWHT is 29 minutes & same is calculated from one hour per inch.

Also please note, the minimum 15 minutes in code, is for only if your value for minimum soaking time(after calculating from one hour per inch for respective thickness) is less than 15 minutes, for eg if you get 14 minutes then you should consider minimum 15 minutes.


Regards


On Monday, 29 May 2017 15:33:46 UTC+5:30, SWI wrote:
Hi Team,

Could any please clarify
What is the minimum required soaking time for P1 material with wall thick 12mm, as per ASME B31.3 year 2014 Table 331.1.1 .

Is it still Minimum one hour per 1 Inch wall thickness or Minimum 15 Minutes...


Regards,

Ram

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...