Friday, May 19, 2017

[MW:26525] duplex contamination

dear expert ;

we have a duplex line connected to pump , the support of thisline is
in carbon steel , for alignement we put a stainless steel shim plate
between support and piping the shim plate is welded to support with
good filler metal ( stainless steel - carbon steel ).

My question is : the duplex will be contaminated or no ?

regards 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...