Re: [MW:25170] Multiple welders can weld in a single production joint?

If they are qualified yes. It happens very often when ‎a welder performs root with GTAW and then an other completes with SMAW

Sent from my BlackBerry 10 smartphone.
From: Rajakani A
Sent: Σάββατο, 30 Ιουλίου 2016 - 09:38
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:25157] Multiple welders can weld in a single production joint?

Dear friends,


 Can multiple welders weld in a single production joint in same process and position?

Kindly clarify me with reference ASME standards if any.

Regards,

Rajakani A,
L&T Construction,
Surat.
+91-7874201744.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...