Dear Sir, 

Take RT/UT of that area (consider the weld area of fillet weld for RF pad also)

After getting it cleared in RT/UT; flush grind the area and do the fitup of the RF pad.

Some specification insists to do DPT after flush grinding (Even after acceptance of RT/UT); before fitup of RF pad.

Regards,

Hareesh K V
+91-8547859202



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: JIJILAL K M <jijilalkm2@gmail.com>
Date: 30/07/2016 2:23 p.m. (GMT+05:30)
To: materials-welding@googlegroups.com
Subject: [MW:25163] RF pad clashing with circumferential pipe weld joints

Dear Experts,

Refer to subject line and attachment , An RF pad is coming closely  with the circumferential weld of a lateral Tee.

Please advice how to resolve it. Code is ASME B 31.1.



Best Regards,

JIJILAL K.M. 
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjWb9xPp0KfV_gBBZh2Xu3Cm33QVuu8TjPAVW_SFmBUsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...