I would strongly recommend NOT USE socket welds in H2S service. The risk of crevice corrosion is to high

Sent from my BlackBerry 10 smartphone.
From: 'Mostafa Kamel Hussein' via Materials & Welding
Sent: Σάββατο, 23 Ιουλίου 2016 - 13:34
To: Materials-welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:25139] PWHT For H2S Socket Weld

Dear Sirs
Kindly be informed our specification mandates PWHT on H2S piping classes regardless its material type except on socket weld  up to 8mm (wall thickness). my question is what is meant by wall thickness? is it base metal thickness of throat thickness? as you know it'll be differed because thickness of fitting is higher than piping thickness in same schedule.
Kindly clarify the meaning and support us with strong evidence if found.
Inline image

Regards,
M.Kamel


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/788535870.3474685.1469263181003.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...