'Runner plates' are metal extensions which are sometimes attached to the top of vertical seams or vertical  weld test plates. These runner plates are generally  called  'Runoff' plates. They will not be specified in the weld / job specifications or codes. They are used by 'experieced' welders who want to prevent the large weld crater or shallow area that comes when a welder terminates his vertical weld at the end of the plates. The runoff plate is generally tack welded to the top back side of the vertical seam being welded. It generally extends 3-6 in. above the top of the test plates. The welder then can continue his weld upward
beyond the 'terminus' of the vertical plates on to the 'Runoff or Runner plate thereby assuring the 'terminus' will be full of metal and not shallow. When the weld
is completed the welder will simply grind off the runoff plate assuring the top is full of weld metal and not shallow. This is very important in welding the multiple plates of a pressure vessel or tank. I hope this explanation will be of benefit to you.
Sincerely,
Gene Matsko
GEM Weld / Materials Consulting Ltd


From: Alan Denney <alan@denney1.freeserve.co.uk>
To: materials-welding@googlegroups.com
Sent: Saturday, July 16, 2016 8:27 AM
Subject: [MW:25108] RE: 25105] runner plates

 
Alan Denney
AKD Materials Consulting Ltd
 
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of shaik amjad
Sent: 16 July 2016 06:31
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25105] runner plates
 
Greetings
 
what is significance of runner plates in structural welding, and the how they are used.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b55bfb2f-83e1-4e4b-9cfa-070edd37177e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000801d1df65%24d1520780%2473f61680%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...