Re: [MW:25106] PWHT

After PWHT, if the welding is added , that means  you have to discard residual stresses which occured  due to additional  welding.
Hence, you have to go for Re-PWHT , refernce ASME 31.3

On 15 July 2016 at 01:41, Krisanu Bhunia <krisanu.bunty@gmail.com> wrote:
Dear sir,

In clean out door in tank we found welding not sufficient after PWHT.(A 537 CL1)
SO, now need to welding again . PWHT again doing or can avoid it by which code ?

Regards
krisanu bhunia
 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMZth3qmH8a3w0Efd96-M12HsymvR61YRPz18j1nOFpdZME9PQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMXKe_rAhWor%2B-ESFSSYX9sJ3-G1vJBLwCf3b0rjNN_uAJHaQA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...