Re: [MW:25096] Type of metal transfer

just a question out of curiosity!

what do we do with knowing type of metal transfer or where is this data used?

is it possible that, with the same parameters, with different welders, the type of transfer is different?

sincerely,
abdulkadir

On Mon, Jul 11, 2016 at 3:53 PM, udaya bhaskar <dusroni@gmail.com> wrote:

sir what you are said that is for low thickness up to 3 mm we were used dip or short circuit transfer, but here at 40 thk

On Jul 11, 2016 14:27, "Alan Denney" <alan@denney1.freeserve.co.uk> wrote:

Correction: generally we use short circuit transfer.

 

Alan Denney

 

 

From: zs00765@rediffmail.com [mailto:zs00765@rediffmail.com]
Sent: 10 July 2016 08:08
To: materials-welding@googlegroups.com
Subject: Re: [MW:25080] Type of metal transfer

 

Dear
There are three types of metal transfer.
Short circuit ... Lower voltage...18-20v
Globular... Medium voltage ... 20 _24v
Spray... Above 24v all are approximately.

Generally in welding we adopt globular or spray transfer.

Sent from RediffmailNG on Android

From: "udaya bhaskar"dusroni@gmail.com
Sent:Sun, 10 Jul 2016 11:54:01 +0530
To: materials-welding@googlegroups.com
Subject: [MW:25079] Type of metal transfer


Hi dear all,


>

PLEASE CLARIFY IN WHICH MODE OF METAL TRANSFER WE DONE  WELDING ? .


>

FOR WPS

 

MATERIAL : IS2062 E250BR


>

THICKNESS: 40 mm


>

PROCESS : GMAW(MAG)


>

GAS          : 100 % CO2


>

MODE OF METAL TRANSFER : ?

--
>

With Regards


>

Udyabahaskar.D


>

--
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3ROShqy3BJdZ57HboYJEpZ9jo1Lq%3DDMJzHoRQfGVyBm4Bg%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1468131841.S.10149.26987.f5-224-116.1468134487.21063%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000f01d1db0d%24e868b8d0%24b93a2a70%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM52_aFM943RcnS1C5U-JUJmvzGmonvt-mtwjjq1P7XMw%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BWqhKeSZ6BiBw03Cvu62qBmL5qPqfs7qE%2BaX6t23oF7%2BQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...