Dear Bhaskar,
You can refer the below standard for EN design vessels.
PD 5500:2015 Specification for unfired fusion welded pressure vessels
Regards,
Saravanan
On Sun, Jul 10, 2016 at 5:49 PM, udaya bhaskar <dusroni@gmail.com> wrote:
Dear all,--Post weld Heat treatment (S.R) code for welds as perASME : Sec VIII Dev 1 under table UCS 56code as per EN Std what ?--With RegardsUdyabahaskar.D+919951728551
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RO-e4AadUntT_xsjnweODS9H0km06bhSJSoNeYWYZaw4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2B_EDQiWaKr0rGChtPKXEL9MVBv6%2BAydAfqY%3DGzPNakHA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments