Re: [MW:25091] Is Joint design is an factor for Ultrasonic testing?

Refer ASME Sec V article 4, Table T-421, weld configurations to be examined is an Essential variable.
Hence you need different calibration blocks for different joint geometries.

PREM S NAUTIYAL
CELL : 9769316004


From: Aakash <harenathjha@gmail.com>
Sent: Mon, 11 Jul 2016 18:45:55
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25087] Is Joint design is an factor for Ultrasonic testing?
Hello,
 Can different weld joint design need different calibration block ?

Please provide refrence litrature.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e253cddb-e88b-4819-a63c-293021248e73@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



Get a professional email for your business Know more >

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1468242955.S.7596.8285.f4-235-148.1468257532.7263%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...