  1) If it is Butt joint: For Root Run GMAW- S ( Short Circuit mode)  followed by Spray or globular mode.
       a) There is separate Miller machine having capability to perform the GMAW process- Short Circuit Mode followed by Globular/ Spray Mode. The same machine you can use it for FCAW- Spray Mode. This Miller-GMAW machine is based on RMD (Regulated Machine Deposition) technique.
      Consumable: Metal Core/ Solid wire both are suitable.
      
       b) Also Lincoln is having separate machine set up to perform the GMAW-S with Short Circuit Mode for root run only and followed by any other process for filling. This Lincoln-GMAW-S based on STT (Surface Tension Transfer) technique.
      Consumable: Only Solid wire.

  2) If WPS as per ASME Sec.IX: Follow QW 403.10.


Regards,
Pravin Nimbalkar
Welding Engineer
BILFAL heavy Industries Ltd. Kingdom of Saudi Arabia.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/710ed520-044f-4c19-85b5-7c7f328d2ea0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...