Wednesday, July 20, 2016

[MW:25126] PWHT

Dear experts

My query is what happens if the soaking time during PWHT is increased beyond the specified minimum time. I know section 8 days minimum soaking time only.

Suppose if required soaking time is 2.5 hours and actual soaking time is 5 hours

Regards
Ishwar Dhiman
Cswip 3.1,ASNT NDT Level-II

Sent from my iPhone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2888C0BE-2391-482F-95BA-0A98DEA102FE%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...