Mr. Pandithan,

 

PWHT is an essential variable for any welding procedure. Hence incorporating 2 PQR’s in one WPS with PWHT & No-PWHT could be confusing. Advice would be to make 2 separate Welding Procedures referencing 2 separate PQR’s . Please look under QW-407 for explanations.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kannayeram Gnanapandithan
Sent: Friday, July 15, 2016 12:13 AM
To: materials-welding
Subject: [MW:25104] ASME Section 9

 

Having 2 PQRs ,one with PWHT and another without PWHT. With these 2 PQRS, can a single WPS be made addressing both conditions by keeping other variable in the order..


THANKS & BEST REGARDS,

KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,

CONSULTANT-WELDING & QUALITY

Mobile no: +919940739349

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO%3DEaB2TgXQB8Usw52QYPOdFDvP_9ZrGPkUJNLKSdL%3DLQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...