Monday, July 11, 2016

[MW:25090] Welding of AISI4130 material with 35CrMo material

Hi Friends,
 
I have requirement for welding of AISI 4130 material with 35CrMo material using GMAW Process.
Whether anybody can provide me the welding Filler wire detail and PWHT detail for this combination.
 
Thanks and Regards,
 
M. Sivachidambaram
QHSE Engineer.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMXCqBLMdbMgEyL-%3DER67h2py_K3LJoBZBLcETaUCUQoGg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...