Dear Mohit,

Yes, you can use FCAW process for stainless steel welding.
The percentage of CO2 you can use 99.995%.

Best Regards,
Chandra
Welding Engineer

On 14-May-2016, at 11:48 AM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

Dear Experts,

Kindly let me know whether FCAW can be used in SS or not and if we can use then how much percentage of CO2 gas should be .

Regards,
Mohit Aggarwal

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPMcfhbT5UA_EChGO-eovO9rGQDWS4Zg3o1u_F7CV5O_TQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...