Refer ASME IX QW 451.4

On Mon, May 2, 2016 at 11:34 PM, <vnbhatt@gmail.com> wrote:
Gents,

We have a 24" pipe rolled from SA 516 Gr 70, 6 mm thick as the pressure inside is 1.2 kg/ cm2 at 423 degree C flue gases.
For support we are welding saddle (RF pad) of IS 2062 Gr A, 8 mm thick. Theoretically it is CS to CS welding. Question is does our CS to CS WPS PQR okay or we need to create one

Highly appreciate useful guidance.

Regards,

Vinod Bhatt.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F5DA11CD-A70D-463B-90C5-91C798C808E9%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABxZsvamEq2QTnu7axpvyxibH57vjYfQsUOm%3D0gNMByJRCLqVw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone