Dear
As per ASME Sec. IX, Table QW-453 there are two types of Overlay (1) Corrosion Resistance (2) Hard Facing. So, 1st you decide types of Overlay and then follow notes no given in Table QW 453.
On Wednesday, May 18, 2016 at 10:04:40 AM UTC+5:30, hoot.1...@gmail.com wrote:
-- As per ASME Sec. IX, Table QW-453 there are two types of Overlay (1) Corrosion Resistance (2) Hard Facing. So, 1st you decide types of Overlay and then follow notes no given in Table QW 453.
On Wednesday, May 18, 2016 at 10:04:40 AM UTC+5:30, hoot.1...@gmail.com wrote:
i am preparing WPS and PQR for overlay for the first time. i have checked ASMEIX QW-453. it just confused me!!!!actually we are finding which materials is the most suitable one for overlaying. the base metal is A216 WCB and the overlay arestellite, monel, F316 and 13%Cr.i read that the dimentions of base metal should be 15*15 cm, with 2.5cm thickness. which examinations should be done on samples to prepare PQR? PT, chemical analysis, hardness nad macro? are these enough?can somebody send me a sample of PQR and WPS for overlay please.best regardssara
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/144f5320-2f4f-4ee6-b0c6-186d989e4394%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments