Wednesday, May 4, 2016

[MW:24757] Regarding improvement in weld quality

Dear Experts,

Kindly give suggestions to improve weld quality for the attached Welding picture.

Material is SA 240 TP 304
Thk 5mm
Process GTAW, Tungsten dia 2.4 mm, Current 148 amperes. Gas Flow Rate 12-15  LPM.

Regards,
Mohit.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPPw3HneemWP1JoqEVKrCtB4-WoFKhaCGi3v7pLkz0mrRw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone