Dear Experts,
     I'm facing high rejection rate because of Tig process ER70S-3. We changed two brands of manufacturer
1.ESAB
2.Metrode
And we done so many test pieces for testing.The type of repairs are mostly inclusions and some porosities.we take many steps to control,still it was continuing.
Guys pls advise to avoid this kind of repairs.
Welders are complaining that there's some slag during welding and it was moving end of the weld pool.it was entrapping on the deposited weld metal and it can't be identified during grinding.we removed copper coating also.but it can't he controlled.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABMP0bMadJa8SejiwLpg9n%2BMw8Bs_b%3D-%2BuazC1QBsUJO4DLQdQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...