Re: [MW:22873] Acceptance of PMI

For the tolerance on obtained element analysis below standards with relevant para may be referred to resolve the issue.

1. ASME Sec I - Appendix B, para B8.2  (± 10% of standard figure)
2. ASTM A 751 (Tolerance on product analysis) 
3. PFI ES 24 (Para 9.3.1 & 9.3.2).- (± 10 for Base metal & ±12.5 for weld metal)

Regds/Jignesh

On Friday, 13 February 2015 09:41:49 UTC+5:30, pradipsil wrote:
Follow PFS standard, 10% bilateral tolerance on parent material & 12.5 % tolerance  on weld material. 
Chk composition on ASME SEC II

On Fri, Feb 13, 2015 at 5:12 AM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

Dear Experts,

We have done PMION weld joint of INCONEL625 i.e. ENiCrMo-3
Found
Ni -61, Cr-24.6, 25.6, Mo-8.5, Nb -3.37,

Now, As per procedure & code i. e.
Sec II C Cr range is 20-23 given
all other elements are in range.
And PMI analyzer also display Inconel 625.
Please confirm whether it is acceptable or not i.e. chromium %

Best Regards,
Mohit Aggarwal.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPOtBHVu5HvuVxdG24WR3uCSsH5sXQkAGkf7C1eLug-r0A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4ba216ce-f69f-4542-bd1e-0609736091e7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...