Monday, February 16, 2015

Re: Fw: [MW:22886] Rechniques for checking internal surface of piping 12" and 16" for natural gas supply

for a continuous pipeline you can use LRUT online and again boroscope offline.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,
 API653, NACE CIP-2, LEEA Registered Engineer.

On Mon, Feb 16, 2015 at 8:50 AM, Mohammed Ghani <ghani386@gmail.com> wrote:
Dear,

its a 40 mtr. continous in service pipe line. i need two options.

1. with out shutdown any chances of internal surface inspection?.
2. with shutdown what are the various types of instruments available for checking internal surface of piping of 40 mtr. length.

Thanks and Regards,
Mohammed Ghani.

On Mon, Feb 16, 2015 at 7:00 AM, 'smkabeer ahamed' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear friend,

snake eye -iii is one type of instrument  used to check internal surface defects,welding defects.vt-level-ii engineers used that instrument.you can approach ndt agency to collect  that instrument and inspect that piping.

Thanks and regards.

S.M.Kabeer ahamed
chief engineer
M/S.QUEST -BANGALURU
INDIA


On Monday, 16 February 2015 8:41 AM, Kunal Patel <kunal.patel13683@gmail.com> wrote:


Dear friend,

For checking internal surface of piping, we can use Borescope or Fiberscope. This is an instrument, which is available in market or vendor places.

Regards,
Kunal Patel
BVIS Ahmedabad.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2a5bc249-f4b9-4c05-9b56-db67ce9d0598%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/101087077.2960395.1424059210045.JavaMail.yahoo%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjNPvBL%2Bi%2BAo1_rQBdrCxfsd0cdVPwu1%2BxO3C5UmeMjmA%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKygcK6UwQsfp6uNvZ0q4F%3DzfgROc2_0G5r2OHNx5q3q7pw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...