Re: [MW:22919] Welding rod for EN 1.7221 material

Dear manivannam,

thanks for advice , but the rod is nickel based , and the e1.7221 chemistry there is no nickel , its chromium based ,

Thanks,
Ambrish

On Monday, February 23, 2015 at 6:38:47 PM UTC+4, manivannan hemu wrote:
Dear Ambrish,

For SMAW You can select E 8016 C1.

Regards,
MANIVANNAN



On Sun, Feb 22, 2015 at 11:34 AM, ambrish dubey <ambr...@gmail.com> wrote:
Dear All,
can anybody help me to decide which filler material is suitable for welding EN1.7221 material

Thanks,
Ambrish

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0a135847-c3f6-4949-8e56-fae1cb3673c9%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e483d983-f8dc-4511-8fac-759110ab4f1f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...