[MW:22915] RE: 22914] welding techniques on pipe spools-reg

Hi friend,
Please elaborate...
What kind of valve, and what is moc, and what kind of packing / gland is their in valve.
Most of the valve manufacturer will give moc of packing to suit to welding only.
Please keep the valve in open condition.
Also maintain some gap at the pipe end(don't touch to valve end).


Lakshman kumar.B
Project manager.
9440031459

From: Siva Chidambaram
Sent: ‎22-‎02-‎2015 12:40
To: materials-welding@googlegroups.com
Subject: [MW:22914] welding techniques on pipe spools-reg

Hi friends,
 
I need some welding techniques for the below issue.
we have pipe spools of 1"& 3/4" with pipe to valves.
Can any body suggest me, how to prepare for welding with pipe to valve.
All joints are socket welds.
1. whether I have to keep the valve in open or closed condition?
2. whether I have to remove the gland from the valves during welding?
 
Kindly suggest me, if there is any procedure for this process?
 
Thanks and regards,
M. Sivachidambaram
QHSE Engineer

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMXin8C_OX%3DVkx4%2Br5MSaCJfo68N3NUysxxam7mhAUpe%3Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...