Monday, February 9, 2015

Re: [MW:22831] High rejection rate in Tig process by using ER 70S-3

dear Sir;

You weld is done according a WPS ?? 
To avoid this kind of defects please check your tungstene electrod and the gas concentration ( 99 % ) any defect in the gas tubing is a problem .

regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258


Le Samedi 7 février 2015 16h59, Srini Vasan <srinicwi@gmail.com> a écrit :


All machines are calibrated also brand-new. Mostly 85% of the welders are facing problem.joint design,parameters,joint cleaning everything perfect.as per discussion with welders they are finding some excessive slags(pacman)which is entrapping in the weld metal.during repair excavation we found some brownish color inclusion spreaded on the location.
Is there any technical problem in 70S-3?
Anybody faces these problems previously in your experience?
On Feb 7, 2015 9:23 AM, "S.Mohammed" <mohd52100@gmail.com> wrote:
1.check your machine calubration or recalibrate.
2.Use ER 70S2.
3.ensure good wind shield.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/69b4bf21-da83-447f-b1df-e6636bfb4317%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABMP0bNoBrSXAFYc2Rkczs_-T25sjVgSU_Tf_G4En%2BQfYY9XLg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...