Re: [MW:22844] SS piping leaking

It can be both, sensitized 304 in high chloride environment


best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Kumar ---11/02/2015 05:52:51---Dear experts, 3" size SS piping (sa 312 tp 304) is found as leaking in few places (near

From: Kumar <sk7920541@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Date: 11/02/2015 05:52
Subject: [MW:22842] SS piping leaking
Sent by: materials-welding@googlegroups.com





Dear experts,
3" size SS piping (sa 312 tp 304) is found as leaking in few places (near to weld joint, base pipe area etc..).the service is potable water.sub- contractor saying it might be due to high chloride content (830ppm) or  defective material (leaks mostly found in 1 heat no.).which could be more relevant? If for material, what are the tests for confirmations?  Kindly share your views.
Thanks in advance,
Kumar.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CALuBtp-W2fmNQjGMZbaQruOAL7pExs1N4fn8ZNzfQ%3DdHsJOAdg%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...