Any idea about Image Contract Graph, In Shell Dep mentioned about excess penetration measurement by Image contrast graph,

Regards,

K.Sundar Rajan

On 22 February 2015 at 09:28, Prashun Kumar <prashunk@gmail.com> wrote:
Excess penentration is measured edge of the joint to base metal in superimposed method by scale.
 
Regards,
 
Prashun

On Sat, Feb 21, 2015 at 9:03 PM, sundarrajan kumaraswamy <ksraja15@gmail.com> wrote:
Dear Pratish,

UT measurement on small bore piping is very difficult , more over probe seating on weld is impossible
so please suggest how to measure weld excess penetration by UT

Any idea about Image Contrast Graph,

Regards,

K.Sundar Rajan

On 21 February 2015 at 09:02, <pkkanishk2006@gmail.com> wrote:
Dear Sundar ,

I believe all have given their input and the good one is to do UT or you can go for gauge pigging which could help u to understand if it is excess or not.

Regards
Pratish 

On Wednesday, February 18, 2015 at 1:49:32 AM UTC+5:30, sundarrajan kumaraswamy wrote:
  How to measure the excess penetration from the Radiograph of Small bore piping  DWDI superimpose Radiograph shows low density near the inner wall,
what is acceptance criteria for excess penetration as per ASME B 31.3 code, Please clarify the IMAGE CONTRAST GRAPH method .

Regards,

K.Sundar Rajan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aaa05311-73f1-44c9-8462-7d967518a773%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAALHs9N6BQqbrC7-pHzxC504rMtBncmT-0A20N_rk14Eiz-WOQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7Um4BVunqBjQ6WnT_jeLC2Hk1207nK7gsH4YZLXsB3QZTB%2Bg%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAALHs9O%2BWj%2BzdtFurUVjPmG9kudULqx6AWsvsoupfOQUTwQ3SQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...