I'm also agree with Mr. Okonkwo and Mr. Sergio about the joint detail (6GR for T, K, Y qualification), but in AWS D1.1-2010>4.13.4.1>3>b we could see a requirement for macro etch sections as follow:
(b) Thorough fusion between adjacent layers of weld metal and between weld metal and base metal.
What is your interpretation about "through fusion between weld metal and base metal"? We cann't see any fusion in "A" surface.
However I know, it is very hard or impractical to weld "A" surface specially in greater thickness differences, but the standard has no special comment about the issue.
I hope the standard add a comment that clearly introduce the minimum required depth for sides to be welded and the fusion (e.i. equal to the thinner part or etc.) in both sides.
Regards
On Wed, Feb 11, 2015 at 11:45 PM, Sergio Antonio Muñoz Pinzón <seanmup@gmail.com> wrote:
Agree with Mr Okonkwo, if this macro was taken from a 6GR coupon made for WPS qualification, chamfering does not apply.
Sergio Muñoz
IWE
Http://weld-ing.blogspot.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ba58088e-4a4e-45fb-9430-5ed03445e4a1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer
Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtudS7iRi5w52Fqh3TGby3Eiupm1DGvRRbbcihOYO5ezcA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments