Hi friends,
 
I need some welding techniques for the below issue.
we have pipe spools of 1"& 3/4" with pipe to valves.
Can any body suggest me, how to prepare for welding with pipe to valve.
All joints are socket welds.
1. whether I have to keep the valve in open or closed condition?
2. whether I have to remove the gland from the valves during welding?
 
Kindly suggest me, if there is any procedure for this process?
 
Thanks and regards,
M. Sivachidambaram
QHSE Engineer

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMXin8C_OX%3DVkx4%2Br5MSaCJfo68N3NUysxxam7mhAUpe%3Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...