RE: [MW:22898] Rechniques for checking internal surface of piping 12" and 16" for natural gas supply

Hello

 

You can use a NDT technique called ultrasound guided waves (UTGW)

 

This technique can detect a serious kind of defects in pipelines, internal and external. Depending of pipe conditions, this NDT can inspect even 50 meters of pipeline in just one test.

 

As is based in ultrasonic principle, this use longitudinal and torsional waves to detect indications which are categorized quantifying the transversal loss of area in pipe. As complement, then you can use single beam of ultrasonic thickness measure to check any indication

 

This can be used with pipeline in service

 

Attached you can find a little information about this NDT

 

There are a lot of services in NDT which offer this one

 

Regards     

 

Miroslav Tadic
Ingeniero  de Integridad
CEE
Gerencia de Producción - Mantenimiento
YPFB Chaco S.A.

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de Mohammed Ghani
Enviado el: domingo, 15 de febrero de 2015 08:13
Para: materials-welding@googlegroups.com
Asunto: [MW:22880] Rechniques for checking internal surface of piping 12" and 16" for natural gas supply

 

Dear Experts,

 

please let me know there is any technique available for checking internal surface of piping (in service fuel natural gas)

 

And also if there is nay technique for checking internal surface of piping during shutdown please let me know.

Thanks and Regards, ?


Mohammed Ghani,

 

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

 

Mechanical Inspector,

BUREAU VERITAS.

 


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVgdiQ8QOm4NMuVuOoVMKP%3DWq5Zt_WZLnQVV7bRUV9mANQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...