Re: [MW:22853] Verification of NACE materials

Dear Mr Vasan,
 
CS materials can also be use for NACE materials, the different will be on the material selection with respect to Chemical Composition and the level of testing as required in NACE M0175
 
Regards,
 
Rems Okonkwo
IWE Nigeria
On Fri, Feb 6, 2015 at 4:59 PM, Srini Vasan <srinicwi@gmail.com> wrote:

Dear Expert's,
           How we can differentiate CS materials and NACE materials when we stake cumulatively?
GA E-60021 what's this coding in the materials?
If it is a traceability means,is it mandatory on the materials?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABMP0bNO_DU%2BiuexRXOe-4GD6%2B8dfdrgVb9WddKcGLchGcfR-A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEpWm6uM%2BwoP_-uaOBt0Kh1k2GtxaQ3JhQx39Oww1cdL9A0AdA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...