These all are the reasons, evaluation of excess penetration using RT for pipes, is never referenced in any codes.
ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,
Nandesh Kumar Arasappa
P.S. : Please don't print this e-mail unless you really need to.
--------------------------------------------
On Wed, 18/2/15, S.Mohammed <mohd52100@gmail.com> wrote:
Subject: Re: [MW:22899] Excess penetration measurment in Radiograph
To: materials-welding@googlegroups.com
Date: Wednesday, 18 February, 2015, 5:45 PM
from where to arrange
ball?
is there standard
size available?
--
You received this message because you are
subscribed to the Google Groups "Materials &
Welding" group.
To unsubscribe from
this group and stop receiving emails from it, send an email
to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/77bec4cf-1331-47d0-acd4-2011d230fc2e%40googlegroups.com.
For
more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1424277311.91425.YahooMailBasic%40web193606.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment