Fw: [MW:22882] Rechniques for checking internal surface of piping 12" and 16" for natural gas supply

Dear friend,

snake eye -iii is one type of instrument  used to check internal surface defects,welding defects.vt-level-ii engineers used that instrument.you can approach ndt agency to collect  that instrument and inspect that piping.

Thanks and regards.

S.M.Kabeer ahamed
chief engineer
M/S.QUEST -BANGALURU
INDIA


On Monday, 16 February 2015 8:41 AM, Kunal Patel <kunal.patel13683@gmail.com> wrote:


Dear friend,

For checking internal surface of piping, we can use Borescope or Fiberscope. This is an instrument, which is available in market or vendor places.

Regards,
Kunal Patel
BVIS Ahmedabad.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2a5bc249-f4b9-4c05-9b56-db67ce9d0598%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...