Re: [MW:22855] IS IT POSSIBLE TO MAKE SPLIT TEE BY CUTTING ORDINARY TEE

Dear Afzal,
 
Need further details about the pupose of spilt tee.
 
In gneral if you want to use the splilt tee for hottap/tie-in purpose you need to split in horizondal portion of the tee.
Moreover, if your want to use the spilt tee over the pipe you cann't able fit it properly due to ID of the tee will not match with OD of the pipe and also you will find gap between halfs after fit-up.
 
Welding & NDT:
 
In case of welding Spilt tee over the pipe, it will be welded with backing strips.
 
Root/first pass - DPI
Final - MPI
Test - Hydrotest of stub.
 
 

 
On Mon, Feb 9, 2015 at 11:14 AM, afzal ahmed <afzalahmed999@gmail.com> wrote:
Dear Friends please Help me ,
 
We need Split Tee of 6"(SMLS SCH 40 ASTM A234 GR WPB) , but it is not available in market easily ,
1: Is it possible to make Split Tee by cutting ordinary Tee vertically
2: if Yes, then in which STD it is telling
3: & what are the NDT requirements
 
for more clarification See the attached file
 
its very urgent .....
 
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0656b478-8126-4723-92b4-e58408747f3b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
With Regards,

Mohan, Q8.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALg_OCxoWToxFuVqGti%3DjnhNOgFHF6a76YjurgjZfEx7NJWyYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...