Monday, February 9, 2015

Re: [MW:22830] Welder Qualification

Dear Sir;

You should ask your client first or check the contract but usually this welder must be qualified according ASME IX.

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258


Le Lundi 9 février 2015 9h43, meisam shokri arfaei <meisamshokri@gmail.com> a écrit :


The first and main document should be used as a reference is a contract. If it mentioned in the contract documents, there is no problem. You will find the acceptable codes, standards, specs., procedures and any other guideline in those documents.

But generally in case of any conflict, the procedure cancels the spec, and the spec cancels the code or standard. Because the procedures have more details and adaptation compare to specs and specs also have more details and adaptation compare to codes and standards.

Regards

On Mon, Feb 9, 2015 at 10:51 AM, Ludmila MANUEL <ludmila.manuel@total.com> wrote:
Dear experts,
 
Please can you give me your advise
 
Can I accept a job in process (Process piping) ASME B31.3 and spec ask for welder qualification as per ASME IX and the welder is qualified as API 1104 (Pipelines)
 
Is there any restriction?
 
thanks
 
 
Ludmila MANUEL
QC Inspector
TOTAL E&P ANGOLA
DT/EPT/ MHSAQ/QUA
Tel : +244 222 67 3443
Cell:+244 912 641 670
Email:
ludmila.Manuel@total.com
 trait (logo).jpg
logo.jpg
Mailing Address:
TOTAL E&P Angola
Rua 6 IL 6 B.I SONILS, Boavista Office B.I 100-01
1
Luanda - Angola
 
 
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1B0224B9A78AB34285E27B011195A0469E7D829F26%40AOEPTTA-EG11.main.glb.corp.local.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMts6tFyeBbfW6k2T26783cTAYLbo5w4xg74MNhu-tEjiCA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...